中国有色金属学报(英文版)
中國有色金屬學報(英文版)
중국유색금속학보(영문판)
TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA
2011年
11期
2542-2547
,共6页
王慧敏%闵小波%柴立元%舒余德
王慧敏%閔小波%柴立元%舒餘德
왕혜민%민소파%시립원%서여덕
铁系%生物聚合铁%絮凝剂
鐵繫%生物聚閤鐵%絮凝劑
철계%생물취합철%서응제
ferrite%poly-ferric sulfate%flocculant
研究生物法制备铁系絮凝剂及其影响因素.以FeSO4·7H2O为原料,利用驯化后的氧化亚铁硫杆菌(T.f)在酸性条件下的催化氧化作用制备生物聚合硫酸铁(PFS),并确定最佳制备条件.实验表明:在反应液初始pH值1.5、硫酸铵用量0.5 g/L、初始Fe2+浓度45 9/L、接种量10%、温度30℃时,在转速为120 r/min的恒温水浴摇床中连续培养5~6 d、可以制出pH l.5~2.2、盐基度17.5%~22.7%、全铁含量43.87~45.24 g/L的产品.实验通过处理3种废水来考察其絮凝性能,结果表明:当PFS投加量一定时,COD去除率可达70%以上,脱色率达90%,Zn2+去除率达99%,说明PFS是一种絮凝效果优异的水处理剂.
研究生物法製備鐵繫絮凝劑及其影響因素.以FeSO4·7H2O為原料,利用馴化後的氧化亞鐵硫桿菌(T.f)在痠性條件下的催化氧化作用製備生物聚閤硫痠鐵(PFS),併確定最佳製備條件.實驗錶明:在反應液初始pH值1.5、硫痠銨用量0.5 g/L、初始Fe2+濃度45 9/L、接種量10%、溫度30℃時,在轉速為120 r/min的恆溫水浴搖床中連續培養5~6 d、可以製齣pH l.5~2.2、鹽基度17.5%~22.7%、全鐵含量43.87~45.24 g/L的產品.實驗通過處理3種廢水來攷察其絮凝性能,結果錶明:噹PFS投加量一定時,COD去除率可達70%以上,脫色率達90%,Zn2+去除率達99%,說明PFS是一種絮凝效果優異的水處理劑.
연구생물법제비철계서응제급기영향인소.이FeSO4·7H2O위원료,이용순화후적양화아철류간균(T.f)재산성조건하적최화양화작용제비생물취합류산철(PFS),병학정최가제비조건.실험표명:재반응액초시pH치1.5、류산안용량0.5 g/L、초시Fe2+농도45 9/L、접충량10%、온도30℃시,재전속위120 r/min적항온수욕요상중련속배양5~6 d、가이제출pH l.5~2.2、염기도17.5%~22.7%、전철함량43.87~45.24 g/L적산품.실험통과처리3충폐수래고찰기서응성능,결과표명:당PFS투가량일정시,COD거제솔가체70%이상,탈색솔체90%,Zn2+거제솔체99%,설명PFS시일충서응효과우이적수처리제.
A novel inorganic polymer flocculant,poly-ferric sulfate (BPFS) was prepared by oxidation of ferrous sulfate using domestic Thiobacillus ferrooxidans (T·f) under acid condition.The optimal conditions for the preparation were pH value of 1.5,(NH4)2SO4 dosage of 0.5 g/L,initial Fe2+ concentration of45g/L,inoculum 10%,rotating speed of 120 r/min,reaction time of 5-6 d and reaction temperature of 30 ℃.Under the optimal conditions,the BPFS product with pH value of 1.5-2.2,basicity of 17.5%-22.7% and total iron content of 43.87-45.24 g/L was obtained.The application of the BPFS to three wastewaters was carried out,and the removal efficiencies of COD,decolorization and Zn2+ by BPFS can be reached 70%,90% and 99%,respectively.The result suggests that the BPFS is an excellent flocculant for water treatment.