固相法制备Pb0.955Pr0.03(ZryTi1-y)O3(PPZT1)和Pb1-1.5xPrx(Zr0.54Ti0.46)O3(PPZT2)系压电陶瓷,其中:x=0.02,0.04,0.06,0.08; y=0.51,0.52,0.54,0.56,0.58,0.60.XRD分析表明:PPZT1系统的准同型相界在锆的摩尔分数为55%左右.当锆的摩尔分数为54%,烧结温度为1 240 ℃,保温1 h,能获得优良的性能,其值分别为:d33=420×10-12 C/N; εT33/ε0=2 000;θC=314 ℃;Qm=76;tanδ=2%;Kp=0.53.XRD分析还表明:PPZT2系统已远离相界,组成均在四方铁电相内.尽管PPZT2系统的介电常数很高,其压电性能却低于PPZT1系统.
固相法製備Pb0.955Pr0.03(ZryTi1-y)O3(PPZT1)和Pb1-1.5xPrx(Zr0.54Ti0.46)O3(PPZT2)繫壓電陶瓷,其中:x=0.02,0.04,0.06,0.08; y=0.51,0.52,0.54,0.56,0.58,0.60.XRD分析錶明:PPZT1繫統的準同型相界在鋯的摩爾分數為55%左右.噹鋯的摩爾分數為54%,燒結溫度為1 240 ℃,保溫1 h,能穫得優良的性能,其值分彆為:d33=420×10-12 C/N; εT33/ε0=2 000;θC=314 ℃;Qm=76;tanδ=2%;Kp=0.53.XRD分析還錶明:PPZT2繫統已遠離相界,組成均在四方鐵電相內.儘管PPZT2繫統的介電常數很高,其壓電性能卻低于PPZT1繫統.
고상법제비Pb0.955Pr0.03(ZryTi1-y)O3(PPZT1)화Pb1-1.5xPrx(Zr0.54Ti0.46)O3(PPZT2)계압전도자,기중:x=0.02,0.04,0.06,0.08; y=0.51,0.52,0.54,0.56,0.58,0.60.XRD분석표명:PPZT1계통적준동형상계재고적마이분수위55%좌우.당고적마이분수위54%,소결온도위1 240 ℃,보온1 h,능획득우량적성능,기치분별위:d33=420×10-12 C/N; εT33/ε0=2 000;θC=314 ℃;Qm=76;tanδ=2%;Kp=0.53.XRD분석환표명:PPZT2계통이원리상계,조성균재사방철전상내.진관PPZT2계통적개전상수흔고,기압전성능각저우PPZT1계통.