对新疆某碳质细粒浸染型难选金矿进行选矿试验研究,结果表明,以硫酸铜为活化剂、丁基黄药和丁铵黑药为捕收剂,采用阶段磨矿-阶段浮选的流程,开路试验得到金品位77.42g/t、金回收率63.10%的较好浮选指标。
對新疆某碳質細粒浸染型難選金礦進行選礦試驗研究,結果錶明,以硫痠銅為活化劑、丁基黃藥和丁銨黑藥為捕收劑,採用階段磨礦-階段浮選的流程,開路試驗得到金品位77.42g/t、金迴收率63.10%的較好浮選指標。
대신강모탄질세립침염형난선금광진행선광시험연구,결과표명,이류산동위활화제、정기황약화정안흑약위포수제,채용계단마광-계단부선적류정,개로시험득도금품위77.42g/t、금회수솔63.10%적교호부선지표。
Experimental study was done on beneficiation of a gold mine in Xinjiang which belongs to carbonaceous granule disseminated type hard dressing gold mine. Result indicated: good flotation indexes of grade 77.42g/t , recovery rate 63.10% of gold could get by open line test which adopted stage grinding-stage flotation process and taken copper sulfate as activator, butyl xanthate and ammonium butyl aerofloat as collector.