以钙基膨润土为原料,系统地研究了改型剂种类与用量、 矿浆浓度以及搅拌时间对改型效果的影响。结果表明:以碳酸钠为改型剂,用量为4%, 矿浆浓度15%,搅拌时间为15 min,对膨润土进行钠化改型,效果显著。
以鈣基膨潤土為原料,繫統地研究瞭改型劑種類與用量、 礦漿濃度以及攪拌時間對改型效果的影響。結果錶明:以碳痠鈉為改型劑,用量為4%, 礦漿濃度15%,攪拌時間為15 min,對膨潤土進行鈉化改型,效果顯著。
이개기팽윤토위원료,계통지연구료개형제충류여용량、 광장농도이급교반시간대개형효과적영향。결과표명:이탄산납위개형제,용량위4%, 광장농도15%,교반시간위15 min,대팽윤토진행납화개형,효과현저。
The main technical conditions for modifying of Ca-bentonite with sodium carbonate or sodium compounds were determined. The natural Ca-bentonite was transferred successfully into artificial Na-bentonite by which the chemical and physical properties of Ca-bentonite was improved largely. Moreover, the fa ctors affecting the quality of modifying of Ca-bentonite were also discussed.