TRANSACTIONS OF NONFERROUS METALS SOCIETY OF CHINA
2004年
4期
756-761
,共6页
肖志瑜%柯美元%陈维平%召明%李元元
肖誌瑜%柯美元%陳維平%召明%李元元
초지유%가미원%진유평%소명%리원원
stainless steel powders%warm compaction%die wall lubrication%lubricant
The warm compacting behaviors of four different kinds of stainless steel powders, 304L, 316L, 410L and 430L, were studied. The results show that warm compaction can be applied to stainless steel powders. The green densities and strengths of compacts obtained through warm compaction are generally higher than those obtained through cold compaction. The compacting behaviors in warm compaction and cold compaction are similar.Under the compacting pressure of 700 MPa, the warm compacted densities are 0. 10 - 0.22 g/cm3 higher than the cold compacted ones, and the green strengths are 11.5 %-50 % higher. The optimal warm compacting temperature is 100 - 110 ℃. In the die wall lubricated warm compaction, the optimum internal lubricant content is 0.2%.