蒲建%王敬丰%肖建中%崔昆
蒲建%王敬豐%肖建中%崔昆
포건%왕경봉%초건중%최곤
bulk amorphous alloys%Pd82Si18%glass forming ability%undercooling%critical cooling rate
Bulk amorphous Pd82Si18 alloy with the largest diameter of 8 mm was prepared by water quenching the molten alloy with flux medium in a quartz tube. The calculation result indicates that the bulk Pd82Si18 amorphous alloys have a low critical cooling rate (Rc) of 4.589 K/s or less. The experimental results show that purifying melt may improve glass forming ability(GFA) of undercooled melt, while liquid phase separation (LPS) of undercooled melt will decrease its GFA. There are some differences in crystallization experiments between bulk metallic glass and amorphous ribbons of Pd82Si18 alloys. These include the numbers of exothermic peak, glass transition temperature Tg, crystallization temperature Tx, region of undercooling liquid (ΔT=Tx-Tg) respectively. The links of cooling rates of melt and crystallization of Pd82Si18 amorphous alloys are explored.