通过红外光谱法研究了粉煤灰、陶瓷抛光废渣和煤粉炉渣等硅质固体废物-石灰体系的蒸压反应特性.6种硅质固体废物的红外光谱强吸收区Si-O伸缩振动频率分别为1 103、1 098、1 094、1 091、1 078、1 033 cm~(-1),硅质固体废物-石灰体系在160 ℃和1.2 MPa饱和蒸汽压下蒸压养护.结果表明,Si-O伸缩振动频率越低,其蒸压样品的结合水量越大,Ca(OH)_2参与反应的比例越高,蒸压反应活性越高.单独硅质固体废物经蒸压处理,其傅立叶变换红外光谱(FTIR)显示,强吸收区的Si-O吸收谱带向低频率方向移动,表明其硅氧四面体聚合程度下降,反应活性增加.
通過紅外光譜法研究瞭粉煤灰、陶瓷拋光廢渣和煤粉爐渣等硅質固體廢物-石灰體繫的蒸壓反應特性.6種硅質固體廢物的紅外光譜彊吸收區Si-O伸縮振動頻率分彆為1 103、1 098、1 094、1 091、1 078、1 033 cm~(-1),硅質固體廢物-石灰體繫在160 ℃和1.2 MPa飽和蒸汽壓下蒸壓養護.結果錶明,Si-O伸縮振動頻率越低,其蒸壓樣品的結閤水量越大,Ca(OH)_2參與反應的比例越高,蒸壓反應活性越高.單獨硅質固體廢物經蒸壓處理,其傅立葉變換紅外光譜(FTIR)顯示,彊吸收區的Si-O吸收譜帶嚮低頻率方嚮移動,錶明其硅氧四麵體聚閤程度下降,反應活性增加.
통과홍외광보법연구료분매회、도자포광폐사화매분로사등규질고체폐물-석회체계적증압반응특성.6충규질고체폐물적홍외광보강흡수구Si-O신축진동빈솔분별위1 103、1 098、1 094、1 091、1 078、1 033 cm~(-1),규질고체폐물-석회체계재160 ℃화1.2 MPa포화증기압하증압양호.결과표명,Si-O신축진동빈솔월저,기증압양품적결합수량월대,Ca(OH)_2삼여반응적비례월고,증압반응활성월고.단독규질고체폐물경증압처리,기부립협변환홍외광보(FTIR)현시,강흡수구적Si-O흡수보대향저빈솔방향이동,표명기규양사면체취합정도하강,반응활성증가.
The autoclaved reaction activities of six silicious solid waste-Ca(OH)_2 systems were studied by Fourier transform infrared(FTIR) spectroscopy. Three indices,viz. combined water amount of the hydration product,percentage of consumed Ca(OH)_2 and compressive strength of the product,were used to indicate the autoclaved reaction activity of silicious solid waste. Six silicious solid waste-Ca(OH)_2 systems were autoclaved at 160 ℃ and 1.2 MPa saturated vapor pressure,and their FTIR spectra were measured. The results showed that the Si-O stretching vibration wavenumbers of the IR absorption bands for 4 fly ashs,1 ceramic polishing waste and 1 cinder were 1 103,1 098,1 094,1091,1 078,1 033 cm~(-1),respectively. It was found that while the Si-O stretching vibration wavenumbers descreased from 1 103 to 1 033 cm~(-1),the combined water amount increased from 5.48% to 7.95%,the percentage of consumed Ca(OH)_2 increased from 72% to 94%,and the compressive strength of product increased from 13.9 to 25.8 MPa. Evidently,the Si-O stretching vibration wavenumber of silicious solid waste has a significant correlation with the autoclaved reaction activity,the lower wavenumber,the higher the reaction activity.