针对长坡选矿厂锌浮选尾矿硫砷矿物相互伴生且部分矿物未单体解离的特点,考虑全浮硫化矿,全浮精矿再硫砷分离的原则流程,在硫砷浮选分离过程中采用过氧化氢与腐殖酸钠1:1药剂组合抑制砷矿物,在用量仅为900g/t条件下,硫精矿品位达到44.86%,回收率达到87.88%,硫精矿中砷含量可降低到1%以下。
針對長坡選礦廠鋅浮選尾礦硫砷礦物相互伴生且部分礦物未單體解離的特點,攷慮全浮硫化礦,全浮精礦再硫砷分離的原則流程,在硫砷浮選分離過程中採用過氧化氫與腐殖痠鈉1:1藥劑組閤抑製砷礦物,在用量僅為900g/t條件下,硫精礦品位達到44.86%,迴收率達到87.88%,硫精礦中砷含量可降低到1%以下。
침대장파선광엄자부선미광류신광물상호반생차부분광물미단체해리적특점,고필전부류화광,전부정광재류신분리적원칙류정,재류신부선분리과정중채용과양화경여부식산납1:1약제조합억제신광물,재용량부위900g/t조건하,류정광품위체도44.86%,회수솔체도87.88%,류정광중신함량가강저도1%이하。
In Changpo plant, the arsenic-sulfur minerals were associated with each other and part minerals were not yet hberated m the tailings of zinc sulfides flotation. According to this problem, a new flowsheet was proposed that bulk flotation was firstly adopted, and then the sulfides concentrate was processed for the separation of arsenic-sulfur minerals. In this experiment, a combined agent of hydrogen peroxide and sodium humate (1:1) was used as an arsenic depressant. The results showed when the depressant dosage was 900g/t, desirable indexes could be achieved that the grade and recovery of sulfide concentrate were respectively 44.86% and 87.88%, and the arsenic content could be reduced to below 1%.