SINTERING AND PELLETIZING
2001年
1期
25-27
,共3页
李振国%张玉柱%常久柱%陶文%栾景林
李振國%張玉柱%常久柱%陶文%欒景林
리진국%장옥주%상구주%도문%란경림
烧结矿%碱度%强度%印度粉矿%澳粉矿
燒結礦%堿度%彊度%印度粉礦%澳粉礦
소결광%감도%강도%인도분광%오분광
试验表明:在唐钢原料条件下,碱度1.4~1.7范围内,配加澳粉矿使烧结矿强度和低温还原粉化性能下降,印度粉矿影响不明显;在碱度0.4~0.6范围内,配加印度粉矿和澳粉矿都有利于烧结矿强度的提高。
試驗錶明:在唐鋼原料條件下,堿度1.4~1.7範圍內,配加澳粉礦使燒結礦彊度和低溫還原粉化性能下降,印度粉礦影響不明顯;在堿度0.4~0.6範圍內,配加印度粉礦和澳粉礦都有利于燒結礦彊度的提高。
시험표명:재당강원료조건하,감도1.4~1.7범위내,배가오분광사소결광강도화저온환원분화성능하강,인도분광영향불명현;재감도0.4~0.6범위내,배가인도분광화오분광도유리우소결광강도적제고。
Experiments indicated that under Tanggang material conditions and at the basicity range of 1.4~1.7, the sinter tumbler strength and reduction desintegration properties were worsen as Australian fine ores added ; but at the basicity range of 0.4~0.6,the sinter strength can improved with both adding of Indian fine ores or Australian fine ores.