以丙烯酸丁酯、丙烯酸-2-乙基己酯、醋酸乙烯酯、丙烯酸羟乙酯及丙烯酸为单体,以乙酸乙酯和二甲苯为溶剂,通过自由基溶液聚合制得自交联丙烯酸酯共聚物黏料,经添加聚磷酸铵阻燃剂,得到了具有阻燃功能的丙烯酸酯压敏胶.通过控制引发剂用量和单体配比可改善压敏胶因聚磷酸铵加入后压敏性降低的问题;当丙烯酸丁酯、丙烯酸羟乙酯、醋酸乙烯酯、丙烯酸-2-乙基己酯和丙烯酸的质量比为42.6∶4.2∶8.5∶42.6∶2.1,引发剂和聚磷酸铵用量分别为单体总质量的1.4%、28%时,所得压敏胶阻燃性能和常规性能均与进口阻燃压敏胶BMS 5-133D的性能相当.
以丙烯痠丁酯、丙烯痠-2-乙基己酯、醋痠乙烯酯、丙烯痠羥乙酯及丙烯痠為單體,以乙痠乙酯和二甲苯為溶劑,通過自由基溶液聚閤製得自交聯丙烯痠酯共聚物黏料,經添加聚燐痠銨阻燃劑,得到瞭具有阻燃功能的丙烯痠酯壓敏膠.通過控製引髮劑用量和單體配比可改善壓敏膠因聚燐痠銨加入後壓敏性降低的問題;噹丙烯痠丁酯、丙烯痠羥乙酯、醋痠乙烯酯、丙烯痠-2-乙基己酯和丙烯痠的質量比為42.6∶4.2∶8.5∶42.6∶2.1,引髮劑和聚燐痠銨用量分彆為單體總質量的1.4%、28%時,所得壓敏膠阻燃性能和常規性能均與進口阻燃壓敏膠BMS 5-133D的性能相噹.
이병희산정지、병희산-2-을기기지、작산을희지、병희산간을지급병희산위단체,이을산을지화이갑분위용제,통과자유기용액취합제득자교련병희산지공취물점료,경첨가취린산안조연제,득도료구유조연공능적병희산지압민효.통과공제인발제용량화단체배비가개선압민효인취린산안가입후압민성강저적문제;당병희산정지、병희산간을지、작산을희지、병희산-2-을기기지화병희산적질량비위42.6∶4.2∶8.5∶42.6∶2.1,인발제화취린산안용량분별위단체총질량적1.4%、28%시,소득압민효조연성능화상규성능균여진구조연압민효BMS 5-133D적성능상당.
A serial of self cross-linking acrylate pressure sensitive adhesive,based on butyl acrylate (BA),2-ethylhexyl ester (2-EHA),vinyl acetate (VAc),2-hydroxyethyl acrylate(HEA) and acrylic acid (AA) as monomers,xylene and ethyl acetate as solvent,are synthesized by solution polymerization.By adding ammonium polyphosphate as flame retardants a flame retardant acrylate pressure-sensitive adhesive is prepared.The dosage of initiator and monomers has great influence on the cohesiveness of pressure-sensitive adhesive.The addition of flame-retardant can improve the flame retardancy of pressure sensitive adhesive flame,and also enhance the bonding performance.When the mass ratio of BA,2-EHA,VAc,HEA and AA is 42.6∶4.2∶8.5∶42.6∶2.1,and adding the initiator and ammonium polyphosphate as 1.4% and 28%,respectively,of all monomers' mass in them,the prepared pressure sensitive adhesive equals an imported sample,BMS 5-133D,in performance.