材料导报
材料導報
재료도보
MATERIALS REVIEW
2009年
z2期
520-523
,共4页
董亚丽%许富民%张志军%石小磊%谭毅
董亞麗%許富民%張誌軍%石小磊%譚毅
동아려%허부민%장지군%석소뢰%담의
添加剂%高纯Al2O3%烧结
添加劑%高純Al2O3%燒結
첨가제%고순Al2O3%소결
additive%high purity alumina%sinter
以纯Al2O3粉、Mg(NO3)2·6H2O、Y(NO3)3·6H2O为原料,于1500℃、1600℃和1700℃常压制备了高纯Al2O3陶瓷,研究了烧结温度和烧结助剂的含量对Al2 O3陶瓷密度、硬度及微观结构的影响.结果表明,添加剂的作用受烧结温度的影响较大,进而影响了烧结体的硬度.
以純Al2O3粉、Mg(NO3)2·6H2O、Y(NO3)3·6H2O為原料,于1500℃、1600℃和1700℃常壓製備瞭高純Al2O3陶瓷,研究瞭燒結溫度和燒結助劑的含量對Al2 O3陶瓷密度、硬度及微觀結構的影響.結果錶明,添加劑的作用受燒結溫度的影響較大,進而影響瞭燒結體的硬度.
이순Al2O3분、Mg(NO3)2·6H2O、Y(NO3)3·6H2O위원료,우1500℃、1600℃화1700℃상압제비료고순Al2O3도자,연구료소결온도화소결조제적함량대Al2 O3도자밀도、경도급미관결구적영향.결과표명,첨가제적작용수소결온도적영향교대,진이영향료소결체적경도.
Al2O3 ceramics are fabricated using high-purity Al2O3 powder,Mg(NO3)2 · 6H2O, and Y(NO3)3 ·6H2O as the raw material,sintered at 1500℃, 1600℃, 1700℃ without pressure. Effects of sintering temperatures and additives on the final density,hardness and microstructure are studied. The results show that the effects of sintering additives are influenced by sintering temperatures,then hardness is effected.