以甲苯二异氰酸酯(TDI)、聚醚多元醇(F-6)、NaHSO3为原料,合成封端型水性聚氨酯(WPU),并用KH-550对其进行有机硅改性,探讨最佳改性工艺。将改性后的封端型WPU用于织物的抗皱、抗起毛起球整理,并对织物进行SEM扫描,结果显示所得WPU的应用性能较好。
以甲苯二異氰痠酯(TDI)、聚醚多元醇(F-6)、NaHSO3為原料,閤成封耑型水性聚氨酯(WPU),併用KH-550對其進行有機硅改性,探討最佳改性工藝。將改性後的封耑型WPU用于織物的抗皺、抗起毛起毬整理,併對織物進行SEM掃描,結果顯示所得WPU的應用性能較好。
이갑분이이청산지(TDI)、취미다원순(F-6)、NaHSO3위원료,합성봉단형수성취안지(WPU),병용KH-550대기진행유궤규개성,탐토최가개성공예。장개성후적봉단형WPU용우직물적항추、항기모기구정리,병대직물진행SEM소묘,결과현시소득WPU적응용성능교호。
Blocked WPU was synthesized using toluene di socyanate ester (TDI), polyether polyol (F-6) and NaHSO3 as main raw materials. KH-550 was used to silicone-modify WPU and the optimal modification process was discussed. The modified blocked WPU was used in wrinkle resistant and anti-pil ing finish of fab-ric, SEM results showed that the modified blocked WPU had good application performance.