31CrMoV9钢%固溶处理%双细化
31CrMoV9鋼%固溶處理%雙細化
31CrMoV9강%고용처리%쌍세화
31 CrMoV9 steel%solution treating%double-refinement
对31 CrMoV9钢棒料和大型齿圈坯件进行了双细化处理。结果表明,双细化工艺处理可使φ70 mm的棒料完全淬透,高温回火后组织为回火索氏体1级,晶粒度6.5~7.5级,力学性能达到或超过德国相关标准,并解决了含V钢切削性能差的问题。
對31 CrMoV9鋼棒料和大型齒圈坯件進行瞭雙細化處理。結果錶明,雙細化工藝處理可使φ70 mm的棒料完全淬透,高溫迴火後組織為迴火索氏體1級,晶粒度6.5~7.5級,力學性能達到或超過德國相關標準,併解決瞭含V鋼切削性能差的問題。
대31 CrMoV9강봉료화대형치권배건진행료쌍세화처리。결과표명,쌍세화공예처리가사φ70 mm적봉료완전쉬투,고온회화후조직위회화색씨체1급,정립도6.5~7.5급,역학성능체도혹초과덕국상관표준,병해결료함V강절삭성능차적문제。
The bars and heavy gear ring blanks of 31CrMoV9 steel were solution-double-refinement treated.The results show that 70-mm-diam bar can be through hardened , and after high tempering the size class number of the tempered sorbite is 1, and the grain size number is 6.5 to 7.5, the mechanical properties reaching or exceeding those in the Germany standards , and removing cutting ability problem of vanadium-containing steel .