选取苏北地区不同品质的杨木加工剩余物为原料,采用一种我国自主研发出来的新型预浸磨浆系统以及常规的高浓盘磨对比研究不同品质杨木加工剩余物对化学机械法制浆性能的影响。研究结果表明:杨木加工剩余物的质量对制取化机浆的制浆得率、磨浆能耗、纸浆白度及纸浆的强度性能均有不同程度的影响。在相同H2O2用量为7.0%,NaOH用量6.0%条件下,以品质较好的杨木加工剩余物为原料,采用双螺杆新型预浸磨浆系统制得化机浆的得率可达85.6%左右,纸浆白度值81%ISO以上,在游离度为300mlCSF条件下,抗张强度可达到33N.m/g以上;以品质较差的杨木加工剩余物为原料,制浆得率为84.2%,纸浆白度为73%左右,抗张强度为29N.m/g。另外,采用双螺杆新型预浸磨浆系统比采用高浓盘磨制浆磨浆电耗上可节省30%左右,制浆得率、纸浆白度及纸浆的强度性能差异不大。
選取囌北地區不同品質的楊木加工剩餘物為原料,採用一種我國自主研髮齣來的新型預浸磨漿繫統以及常規的高濃盤磨對比研究不同品質楊木加工剩餘物對化學機械法製漿性能的影響。研究結果錶明:楊木加工剩餘物的質量對製取化機漿的製漿得率、磨漿能耗、紙漿白度及紙漿的彊度性能均有不同程度的影響。在相同H2O2用量為7.0%,NaOH用量6.0%條件下,以品質較好的楊木加工剩餘物為原料,採用雙螺桿新型預浸磨漿繫統製得化機漿的得率可達85.6%左右,紙漿白度值81%ISO以上,在遊離度為300mlCSF條件下,抗張彊度可達到33N.m/g以上;以品質較差的楊木加工剩餘物為原料,製漿得率為84.2%,紙漿白度為73%左右,抗張彊度為29N.m/g。另外,採用雙螺桿新型預浸磨漿繫統比採用高濃盤磨製漿磨漿電耗上可節省30%左右,製漿得率、紙漿白度及紙漿的彊度性能差異不大。
선취소북지구불동품질적양목가공잉여물위원료,채용일충아국자주연발출래적신형예침마장계통이급상규적고농반마대비연구불동품질양목가공잉여물대화학궤계법제장성능적영향。연구결과표명:양목가공잉여물적질량대제취화궤장적제장득솔、마장능모、지장백도급지장적강도성능균유불동정도적영향。재상동H2O2용량위7.0%,NaOH용량6.0%조건하,이품질교호적양목가공잉여물위원료,채용쌍라간신형예침마장계통제득화궤장적득솔가체85.6%좌우,지장백도치81%ISO이상,재유리도위300mlCSF조건하,항장강도가체도33N.m/g이상;이품질교차적양목가공잉여물위원료,제장득솔위84.2%,지장백도위73%좌우,항장강도위29N.m/g。령외,채용쌍라간신형예침마장계통비채용고농반마제장마장전모상가절성30%좌우,제장득솔、지장백도급지장적강도성능차이불대。
The effect on chemi-mechanical pulping performance was studied with twin-screw preimpregnating reifner and disc reifner, using poplar wood processing residues from the northern of Jiangsu province as raw material. The results show that the quality of poplar wood processing residues has an impact on pulping yield, specific refining energy, pulp brightness and strength properties. Under the chemical conditions of hydrogen peroxide dosages of 7.0%, combined with 6.0%sodium hydroxide based on oven dry chip, for impregnation, the high quality pulp with brightness levels of 81%ISO or up and the yield of about 85.6% is obtained by twin-screw reifner preimpregnating using high quality poplar wood processing residues. At the freeness level of CSF 300ml, pulp tensile strength can reach to 33N.m/g or up; by using poor quality poplar wood processing residues as raw material, the pulping yield reaches to 84.2%, brightness up to about 73%ISO, tensile index 29N.m/g. Furthermore, 30%speciifc reifning energy can be saved with twin-screw preimpregnating reifner followed by high concentration disc reifner, while the yield of pulping, pulp brightness and pulp strength have only a little difference.