以粉煤灰为原料,采用酸溶、搅拌加热,静置熟化的方法制备了新型无机高分子絮凝剂聚合氯化铝铁。结果表明:絮凝剂制备的最佳提取条件是反应温度为90℃,料液比为5:17,反应时间为1.5h。
以粉煤灰為原料,採用痠溶、攪拌加熱,靜置熟化的方法製備瞭新型無機高分子絮凝劑聚閤氯化鋁鐵。結果錶明:絮凝劑製備的最佳提取條件是反應溫度為90℃,料液比為5:17,反應時間為1.5h。
이분매회위원료,채용산용、교반가열,정치숙화적방법제비료신형무궤고분자서응제취합록화려철。결과표명:서응제제비적최가제취조건시반응온도위90℃,료액비위5:17,반응시간위1.5h。
In this paper, taking fly ash as raw material, it uses the method of acid soluble, stirring to heat up and standing for the maturation to prepare the new type of inorganic polymer flocculants - poly aluminum ferric chloride. The results show that the best extraction conditions of the flocculant preparation: the reaction temperature is 90℃, the proportion between solid material and liquid is 5: 17, and the reaction time is 1.5h.