介绍了羊毛角蛋白膜的制备工艺,对比分析了羊毛和其角蛋白膜的热学性能,得出羊毛的最大失重峰出现在327℃左右,范围在153~550℃;羊毛角蛋白多孔膜的主要失重峰分别在321℃和502℃,失重范围为230~545℃,两者的主要失重峰很接近。
介紹瞭羊毛角蛋白膜的製備工藝,對比分析瞭羊毛和其角蛋白膜的熱學性能,得齣羊毛的最大失重峰齣現在327℃左右,範圍在153~550℃;羊毛角蛋白多孔膜的主要失重峰分彆在321℃和502℃,失重範圍為230~545℃,兩者的主要失重峰很接近。
개소료양모각단백막적제비공예,대비분석료양모화기각단백막적열학성능,득출양모적최대실중봉출현재327℃좌우,범위재153~550℃;양모각단백다공막적주요실중봉분별재321℃화502℃,실중범위위230~545℃,량자적주요실중봉흔접근。
The preparation process of wool keratin membrane were introduced,and the thermal property of wool and wool keratin film was comparative analyzed.The test results showed that the weight loss temperature range of wool was 153~550 ℃,and the maximum weight loss peak appeared at 327 ℃.While the weight loss temperature range of wool keratin membrane was 230~545 ℃,and the main weight loss peaks were 321 ℃ and 502 ℃.The main weight loss peak between wool and wool keratin was much close.