钢板氧炔切割面在电弧喷涂时,容易出现涂层剥落的情况。通过研究发现,Q345B氧割面金相组织由铁素体和珠光体变成了马氏体,硬度提高了一倍,该变化使氧割面很难获得电弧喷涂所需要的粗糙度。单纯的锌铝合金涂层防腐性能并不理想,必须进行封闭处理。
鋼闆氧炔切割麵在電弧噴塗時,容易齣現塗層剝落的情況。通過研究髮現,Q345B氧割麵金相組織由鐵素體和珠光體變成瞭馬氏體,硬度提高瞭一倍,該變化使氧割麵很難穫得電弧噴塗所需要的粗糙度。單純的鋅鋁閤金塗層防腐性能併不理想,必鬚進行封閉處理。
강판양결절할면재전호분도시,용역출현도층박락적정황。통과연구발현,Q345B양할면금상조직유철소체화주광체변성료마씨체,경도제고료일배,해변화사양할면흔난획득전호분도소수요적조조도。단순적자려합금도층방부성능병불이상,필수진행봉폐처리。
When applying electric arc spraying, the coating is easy to peel from the surface of the steel's acetylene cutting face. We found that the metallurgical structures were changed from ferrite and pearlite to martensite and their hardness increased 1 time. This change makes the acetylene cutting face difficult to get the required roughness. The resist-corrosion performance of pure zinc alloy coating is not ideal. The coating must be sealed.