NON-FEROUS MINING AND METALLURGY
2014年
5期
36-37
,共2页
高铜铅精矿%富氧底吹工艺%铅锍%粗铅
高銅鉛精礦%富氧底吹工藝%鉛锍%粗鉛
고동연정광%부양저취공예%연류%조연
high copper lead concentrate%rich oxygen bottom blowing process%lead matte%crude lead
某铅厂处理了一批高铜铅精矿,通过2个月的工业生产,入炉原料含铜高对底吹炉、烟化炉生产有一定影响,整个工业试验结果表明,铜可以在粗铅及锍中富集,粗铅含铜可达10%以上,锍含铜可达40%以上,弃渣含铜可控制在0.65%以下,铜的回收率可达90%。
某鉛廠處理瞭一批高銅鉛精礦,通過2箇月的工業生產,入爐原料含銅高對底吹爐、煙化爐生產有一定影響,整箇工業試驗結果錶明,銅可以在粗鉛及锍中富集,粗鉛含銅可達10%以上,锍含銅可達40%以上,棄渣含銅可控製在0.65%以下,銅的迴收率可達90%。
모연엄처리료일비고동연정광,통과2개월적공업생산,입로원료함동고대저취로、연화로생산유일정영향,정개공업시험결과표명,동가이재조연급류중부집,조연함동가체10%이상,류함동가체40%이상,기사함동가공제재0.65%이하,동적회수솔가체90%。
A lead factory had smelted a batch of high copper content of lead concentrate , through two months of industrial practice , high copper content of lead concentrate had certain influence to the produc-tion of bottom blowing furnace and fuming furnace . The industrial test results showed that copper can be enriched in the crude lead and matte , the copper content of crude lead can reach more than 10 percent , the copper content of matte can reach more than 40 percent , the copper content of slag can be controlled under 0 .65 percent , and the recovery rate of copper can reach more than 90 percent .