张翼%李容%王延松%李书武
張翼%李容%王延鬆%李書武
장익%리용%왕연송%리서무
片麻岩云母%研磨开片%棒磨开片%复合云母纸
片痳巖雲母%研磨開片%棒磨開片%複閤雲母紙
편마암운모%연마개편%봉마개편%복합운모지
gneiss mica%delamination by grinding%delamination by rod milling%composite mica paper
对煅烧的片麻岩云母采用不同的机械开片方式处理后,与伟晶岩云母鳞片混合制得复合云母纸,研究不同开片方式对片麻岩复合云母纸拉伸强度的影响.结果表明:研磨方式更适合于片麻岩云母的开片处理,当研磨开片处理时间为15 min,片麻岩云母掺加量为9%时,复合云母纸的拉伸强度达到最大值4.8 N/cm.
對煅燒的片痳巖雲母採用不同的機械開片方式處理後,與偉晶巖雲母鱗片混閤製得複閤雲母紙,研究不同開片方式對片痳巖複閤雲母紙拉伸彊度的影響.結果錶明:研磨方式更適閤于片痳巖雲母的開片處理,噹研磨開片處理時間為15 min,片痳巖雲母摻加量為9%時,複閤雲母紙的拉伸彊度達到最大值4.8 N/cm.
대단소적편마암운모채용불동적궤계개편방식처리후,여위정암운모린편혼합제득복합운모지,연구불동개편방식대편마암복합운모지랍신강도적영향.결과표명:연마방식경괄합우편마암운모적개편처리,당연마개편처리시간위15 min,편마암운모참가량위9%시,복합운모지적랍신강도체도최대치4.8 N/cm.
A composite mica paper was prepared by mixing calcined gneiss mica treated by different me-chanical delamination method and pegmatite mica, and the effects of different treatments of gneiss mica on the tensile strength of the composite mica paper were studied. The results show that the grinding treat-ment is more suitable for the delamination of gneiss mica. When the grinding time is 15 min, the gneiss mica content is 9% , the tensile strength of the composite mica paper attains its maximum value 4.8 N/cm.