本文针对甘肃省铅锌矿石铅品位较低,铅矿物种类多,嵌布粒度粗细不均等特点,研究采用顺序优先浮选的工艺流程,最终获得了铅精矿品位51.50%,回收率50.31%;锌精矿品位58.10%,锌回收率96.43%的较好选别指标。实现了对该矿山资源的综合回收利用。
本文針對甘肅省鉛鋅礦石鉛品位較低,鉛礦物種類多,嵌佈粒度粗細不均等特點,研究採用順序優先浮選的工藝流程,最終穫得瞭鉛精礦品位51.50%,迴收率50.31%;鋅精礦品位58.10%,鋅迴收率96.43%的較好選彆指標。實現瞭對該礦山資源的綜閤迴收利用。
본문침대감숙성연자광석연품위교저,연광물충류다,감포립도조세불균등특점,연구채용순서우선부선적공예류정,최종획득료연정광품위51.50%,회수솔50.31%;자정광품위58.10%,자회수솔96.43%적교호선별지표。실현료대해광산자원적종합회수이용。
According to the characters of the low grade of the ore, many kinds of lead minerals and uneven dissemination size, the sequential selective flotation process is adopted, finally achieving a grade of 51.50%, a recovery rate of 50.31%for the lead concentrate, a grade of 58.10%, a recovery rate of 96.43%for the Zinc concentrate and realizing the compre-hensive recycling and utilization of the mine resources.