李培中%苏玉虎%孙朝晖%冯明光%蒋雷
李培中%囌玉虎%孫朝暉%馮明光%蔣雷
리배중%소옥호%손조휘%풍명광%장뢰
丙烯球罐%焊接裂纹%分析%修复
丙烯毬罐%銲接裂紋%分析%脩複
병희구관%한접렬문%분석%수복
propylene spherical tank%weld cracks%analysis%repair
对球罐在安装过程中产生的焊接裂纹进行了分析,制定了合理的返修方案。经返修检验,投入使用2年后未发现超标缺陷。
對毬罐在安裝過程中產生的銲接裂紋進行瞭分析,製定瞭閤理的返脩方案。經返脩檢驗,投入使用2年後未髮現超標缺陷。
대구관재안장과정중산생적한접렬문진행료분석,제정료합리적반수방안。경반수검험,투입사용2년후미발현초표결함。
The weld cracks occurred in the process of fabricating 2000 m3 propylene spherical tank were analyzed,and a reasonable repair scheme was formulated based on above analysis.The inspection was car-ried out after repair,there are no over-standard of defects found in the two years operating.