高铜锌精矿%铜回收%浮选
高銅鋅精礦%銅迴收%浮選
고동자정광%동회수%부선
high copper content zinc concentrate%Cu recovery%flotation
为回收高铜锌精矿中的铜,抑锌浮铜试验采用硫酸锌为锌抑制剂,G6和酯10为铜捕收剂,通过调整硫酸锌和G6的用量,选定条件下获得铜品位为26.18%的铜精矿、锌品位为53.38%的锌精矿,铜、锌金属回收率分别为77.50%、98.46%,实现了较好的经济效益和社会效益。
為迴收高銅鋅精礦中的銅,抑鋅浮銅試驗採用硫痠鋅為鋅抑製劑,G6和酯10為銅捕收劑,通過調整硫痠鋅和G6的用量,選定條件下穫得銅品位為26.18%的銅精礦、鋅品位為53.38%的鋅精礦,銅、鋅金屬迴收率分彆為77.50%、98.46%,實現瞭較好的經濟效益和社會效益。
위회수고동자정광중적동,억자부동시험채용류산자위자억제제,G6화지10위동포수제,통과조정류산자화G6적용량,선정조건하획득동품위위26.18%적동정광、자품위위53.38%적자정광,동、자금속회수솔분별위77.50%、98.46%,실현료교호적경제효익화사회효익。
For better Cu flotation recovery from high copper content zinc concentrate, this experiment changes the dosage of depressor ZnSO4 and collector G6, in the optimum conditions, the copper concentrate containing Cu 26.18%, the zinc concentrate containing Zn 53.38%, the recovery of Cu and Zn are 77.50% and 98.46%respectively, reaching a good economic and social benefit.