INTERNATIONAL JOURNAL OF MINERALS,METALLURGY AND MATERIALS
2015年
8期
798-803
,共6页
lead-acid batteries%molten salts%lead smelting%desulfurization%solid waste recycling
Lead extraction from spent lead–acid battery paste in a molten Na2CO3 salt containing ZnO as a sulfur-fixing agent was studied. Some influencing factors, including smelting temperature, reaction time, ZnO and salt dosages, were investigated in detail using single-factor experiments. The optimum conditions were determined as follows:T = 880°C;t = 60 min; Na2CO3/paste mass ratio = 2.8:1; and the ZnO dosage is equal to the stoichiometric requirement. Under the optimum conditions, the direct recovery rate of lead reached 98.14%. The re-sults suggested that increases in temperature and salt dosage improved the direct recovery rate of lead. XRD results and thermodynamic cal-culations indicated that the reaction approaches of lead and sulfur were PbSO4→Pb and PbSO4→ZnS, respectively. Sulfur was fixed in the form of ZnS, whereas the molten salt did not react with other components, serving only as a reaction medium.