传感技术学报
傳感技術學報
전감기술학보
Chinese Journal of Sensors and Actuators
2015年
9期
1292-1296
,共5页
间甲酚紫-PVP复合薄膜%光波导元件%旋转甩涂
間甲酚紫-PVP複閤薄膜%光波導元件%鏇轉甩塗
간갑분자-PVP복합박막%광파도원건%선전솔도
M-Cresol purple-polyvinylpyrrolidone composite film%optical waveguide sensor%spin-coating
利用旋转甩涂法(Spin-Coating)将间甲酚紫-聚乙烯吡咯烷酮复合薄膜固定在K+交换玻璃光波导表面研制了光波导敏感元件.研究了不同复合比例的间甲酚紫-聚乙烯吡咯烷酮复合薄膜与酸性和挥发性有机气体作用前后的紫外可见吸收光谱变化,并在此基础上研究了该敏感元件在光波导测试系统中对酸性和挥发性有机气体的响应.敏感薄膜与酸性气体作用后,薄膜由黄色变为紫红色.该敏感元件能检测到体积比浓度低于1×10-10(1.41×10-4 mg/m3)的H2S,响应和恢复时间分别为1.1 s和8.5 s,信噪比S/N为15.43;能检测到体积比浓度低于1×10-10(2.66×10-4 mg/m3)SO2气体,响应和恢复时间分别为0.4 s和2.7 s,信噪比S/N为5.88.间甲酚紫-聚乙烯吡咯烷酮复合薄膜厚度为199 nm±5 nm.
利用鏇轉甩塗法(Spin-Coating)將間甲酚紫-聚乙烯吡咯烷酮複閤薄膜固定在K+交換玻璃光波導錶麵研製瞭光波導敏感元件.研究瞭不同複閤比例的間甲酚紫-聚乙烯吡咯烷酮複閤薄膜與痠性和揮髮性有機氣體作用前後的紫外可見吸收光譜變化,併在此基礎上研究瞭該敏感元件在光波導測試繫統中對痠性和揮髮性有機氣體的響應.敏感薄膜與痠性氣體作用後,薄膜由黃色變為紫紅色.該敏感元件能檢測到體積比濃度低于1×10-10(1.41×10-4 mg/m3)的H2S,響應和恢複時間分彆為1.1 s和8.5 s,信譟比S/N為15.43;能檢測到體積比濃度低于1×10-10(2.66×10-4 mg/m3)SO2氣體,響應和恢複時間分彆為0.4 s和2.7 s,信譟比S/N為5.88.間甲酚紫-聚乙烯吡咯烷酮複閤薄膜厚度為199 nm±5 nm.
이용선전솔도법(Spin-Coating)장간갑분자-취을희필각완동복합박막고정재K+교환파리광파도표면연제료광파도민감원건.연구료불동복합비례적간갑분자-취을희필각완동복합박막여산성화휘발성유궤기체작용전후적자외가견흡수광보변화,병재차기출상연구료해민감원건재광파도측시계통중대산성화휘발성유궤기체적향응.민감박막여산성기체작용후,박막유황색변위자홍색.해민감원건능검측도체적비농도저우1×10-10(1.41×10-4 mg/m3)적H2S,향응화회복시간분별위1.1 s화8.5 s,신조비S/N위15.43;능검측도체적비농도저우1×10-10(2.66×10-4 mg/m3)SO2기체,향응화회복시간분별위0.4 s화2.7 s,신조비S/N위5.88.간갑분자-취을희필각완동복합박막후도위199 nm±5 nm.
M-cresol purple-polyvinylpyrrolidone(m-CP-PVP)composite film components was fixed on K+glass opti-cal waveguide surface with the method of spin-coating. We studied the UV-visible absorption spectrum variation of the different compound ratio of m-cresol purple-polyvinylpyrrolidone composite film/K+exchange glass optical wave-guide sensor before and after reacting with acidic and volatile organic compounds gases,and on the basis of study-ing the sensor response of acidic and volatile organic compounds gases in the optical waveguide detection system. The sensitive film was changed from yellow to red when it reacted with acidic gases. The sensor can detect H 2S with the volume concentration which is lower than 1×10-10(1.41×10-4 mg/m3),response and recovery time are 1.1 s and 8.5 s,andS/N is 15.43;and SO2 is lower than 1×10-10(2.66×10-4 mg/m3),response and recovery time are 0.4 s and 2.7 s,and S/N is 5.88. Meanwhile,the thickness of m-CP-PVP composite film is 199 nm±5 nm.