采用MLA矿物自动定量检测系统,结合传统的工艺矿物学研究方法,对某钨多金属矿石进行工艺矿物学研究。原矿石含WO31.25%,钨主要以白钨矿和黑钨矿矿物形式存在,理论最高回收率约为99%;铜主要以黄铜矿矿物形式存在,理论最高回收率约为96%;银矿物种类多、含量低,与方铅矿、自然铋等铅铋矿物紧密共生,可从含铅铋矿物的铜精矿中回收银,理论最高回收率约为61%。研究数据表明矿石中的钨矿物主要呈大脉状产出,少数呈细粒浸染状产出,在空间分布和嵌布粒度上极不均匀。白钨矿(含黑钨矿)和黄铜矿的粒度较粗,大于0.04 mm粒级者分别占约95%和73%,对磨矿解离非常有利。
採用MLA礦物自動定量檢測繫統,結閤傳統的工藝礦物學研究方法,對某鎢多金屬礦石進行工藝礦物學研究。原礦石含WO31.25%,鎢主要以白鎢礦和黑鎢礦礦物形式存在,理論最高迴收率約為99%;銅主要以黃銅礦礦物形式存在,理論最高迴收率約為96%;銀礦物種類多、含量低,與方鉛礦、自然鉍等鉛鉍礦物緊密共生,可從含鉛鉍礦物的銅精礦中迴收銀,理論最高迴收率約為61%。研究數據錶明礦石中的鎢礦物主要呈大脈狀產齣,少數呈細粒浸染狀產齣,在空間分佈和嵌佈粒度上極不均勻。白鎢礦(含黑鎢礦)和黃銅礦的粒度較粗,大于0.04 mm粒級者分彆佔約95%和73%,對磨礦解離非常有利。
채용MLA광물자동정량검측계통,결합전통적공예광물학연구방법,대모오다금속광석진행공예광물학연구。원광석함WO31.25%,오주요이백오광화흑오광광물형식존재,이론최고회수솔약위99%;동주요이황동광광물형식존재,이론최고회수솔약위96%;은광물충류다、함량저,여방연광、자연필등연필광물긴밀공생,가종함연필광물적동정광중회수은,이론최고회수솔약위61%。연구수거표명광석중적오광물주요정대맥상산출,소수정세립침염상산출,재공간분포화감포립도상겁불균균。백오광(함흑오광)화황동광적립도교조,대우0.04 mm립급자분별점약95%화73%,대마광해리비상유리。
This paper studies the process mineralogy of a tungsten poly-metallic ore by automatic quantitative mineral technology MLA combined with traditional methods. WO3 grade of the ore is 1.25%, tungsten mainly exists as scheelite and wolframite with theoretical recovery rate attaining 99%;copper chiefly exists as chalcopyrite with theoretical recovery rate reaching 96 %; these silver minerals have many types but low content,closely associated with lead-bismuth minerals such as galena and native bismuth. The theoretica recovery rate can attain 61% if recovering silver from copper concentrate. The results indicate that the tungsten minerals in the ore mainly output as large veins,but a few of them as fine grain-disseminated structure.The spatial distribution and dissemination size of tungsten minerals are extremely uneven.The grain size of scheelite (containing wolframite) and chalcopyrite are relatively coarse and the grain size of more than 0.04 mm accounted for about 95%and 73%respectively, which is very beneficial for grinding dissociation.