西藏某多金属矿选厂的铜钼混合精矿-0.048 mm含量为85%,铜、钼品位分别为19.06%和0.640%,金、银含量分别为6.98和490.90 g/t,99%以上的铜钼矿物为原生或次生硫化矿物。采用高效易降解药剂对该混合精矿进行铜钼分离选矿试验,结果表明,在磨矿细度为-0.048 mm占90%的情况下,以高效易降解的ZG-2为铜矿物抑制剂、HTL-3为钼捕收剂,采用1粗4精2扫、中矿顺序返回的闭路流程分离试样中的铜钼,最终可获得钼品位为47.68%、钼回收率为81.45%的钼精矿,和铜品位为19.26%、铜回收率为99.94%的铜精矿,金、银主要富集在铜精矿中,实现了该铜钼混合精矿的高效、低毒分离。
西藏某多金屬礦選廠的銅鉬混閤精礦-0.048 mm含量為85%,銅、鉬品位分彆為19.06%和0.640%,金、銀含量分彆為6.98和490.90 g/t,99%以上的銅鉬礦物為原生或次生硫化礦物。採用高效易降解藥劑對該混閤精礦進行銅鉬分離選礦試驗,結果錶明,在磨礦細度為-0.048 mm佔90%的情況下,以高效易降解的ZG-2為銅礦物抑製劑、HTL-3為鉬捕收劑,採用1粗4精2掃、中礦順序返迴的閉路流程分離試樣中的銅鉬,最終可穫得鉬品位為47.68%、鉬迴收率為81.45%的鉬精礦,和銅品位為19.26%、銅迴收率為99.94%的銅精礦,金、銀主要富集在銅精礦中,實現瞭該銅鉬混閤精礦的高效、低毒分離。
서장모다금속광선엄적동목혼합정광-0.048 mm함량위85%,동、목품위분별위19.06%화0.640%,금、은함량분별위6.98화490.90 g/t,99%이상적동목광물위원생혹차생류화광물。채용고효역강해약제대해혼합정광진행동목분리선광시험,결과표명,재마광세도위-0.048 mm점90%적정황하,이고효역강해적ZG-2위동광물억제제、HTL-3위목포수제,채용1조4정2소、중광순서반회적폐로류정분리시양중적동목,최종가획득목품위위47.68%、목회수솔위81.45%적목정광,화동품위위19.26%、동회수솔위99.94%적동정광,금、은주요부집재동정광중,실현료해동목혼합정광적고효、저독분리。
Particles of a copper-molybdenum rough concentrate from a polymetallic plant in Tibet is -0. 048 mm 85%. Copper,molybdenum,gold and silver grade is 19. 06%,0. 640%,6. 98 g/t,and 490. 90 g/t,respectively. Over 99% of the copper and molybdenum are native or secondary sulfide minerals. Beneficiation experiments were conducted on the ore in order to separate molybdenum from copper on the mixed concentrate using highly efficient and easy to be degraded reagent. The re-sults indicated that:molybdenum concentrate with molybdenum grade of 47. 68% and recovery of 81. 45%,and copper concen-trate with copper grade of 19. 26% and recovery of 99. 94% was obtained by the process of one roughing-four cleaning-two scavenging and middlings back to the flow-sheet in turn with high efficient and easy to be degraded ZG-2 as copper depressor, HTL-3 as copper collector at the grinding fineness of 0. 048 mm passing 90%. Gold and silver mainly were enriched in copper concentrate. High efficiency and low toxicity separation of the copper-molybdenum bulk concentrate can be achieved.