250A是中国矿业大学新研制的一种新型、价廉、易降解、低污染的选铜起泡剂,为了检验其高效性,以安徽铜陵某低品位原生铜矿石为试样进行了选铜试验。在磨矿细度为-0.074 mm占75%的情况下,以条件试验确定的药剂用量为粗选用量,参照现场工艺流程进行了2种起泡剂的浮选效果对比试验。结果表明:250A总用量为241 g/t的情况下,铜精矿铜品位和铜回收率分别为21.56%和87.32%;松醇油总用量为360 g/t的情况下,铜精矿铜品位和铜回收率分别为21.67%和87.19%。两相比较可知,250A比松醇油更高效,有助于选铜企业降本增效。
250A是中國礦業大學新研製的一種新型、價廉、易降解、低汙染的選銅起泡劑,為瞭檢驗其高效性,以安徽銅陵某低品位原生銅礦石為試樣進行瞭選銅試驗。在磨礦細度為-0.074 mm佔75%的情況下,以條件試驗確定的藥劑用量為粗選用量,參照現場工藝流程進行瞭2種起泡劑的浮選效果對比試驗。結果錶明:250A總用量為241 g/t的情況下,銅精礦銅品位和銅迴收率分彆為21.56%和87.32%;鬆醇油總用量為360 g/t的情況下,銅精礦銅品位和銅迴收率分彆為21.67%和87.19%。兩相比較可知,250A比鬆醇油更高效,有助于選銅企業降本增效。
250A시중국광업대학신연제적일충신형、개렴、역강해、저오염적선동기포제,위료검험기고효성,이안휘동릉모저품위원생동광석위시양진행료선동시험。재마광세도위-0.074 mm점75%적정황하,이조건시험학정적약제용량위조선용량,삼조현장공예류정진행료2충기포제적부선효과대비시험。결과표명:250A총용량위241 g/t적정황하,동정광동품위화동회수솔분별위21.56%화87.32%;송순유총용량위360 g/t적정황하,동정광동품위화동회수솔분별위21.67%화87.19%。량상비교가지,250A비송순유경고효,유조우선동기업강본증효。
The 250A is a new,inexpensive,readily biodegradable,less polluting copper frother which is newly developed by China University of Mining and Technology. To test its efficiency,copper flotation experiment were carried out on a certain low grade copper ore from Tongling in Anhui Province. Under the condition that grinding fineness of -0. 074 mm account for 75%,a condition experiment was carried out to estimated dosage of roughing and a comparative test was carried out to compare flotation effect of two frothers with reference to field process. The results show that,under situation of the total dosage of 250A 100 g/t,copper concentrate contained 21. 56% Cu and recovery rate of 87. 32% was obtained;Correspondingly,under condi-tion of the total dosage of pine camphor oil 150 g/t, the copper concentrates contained 21. 67% Cu and recovery rate of 87. 17% were achieved. Obviously,250A is high efficient and helpful to reduce cost and increase benefit for copper enterprise.